Appearance of craters on the paint surface (interior or exterior)

Discover the potential causes and view the solutions
• Intense shaking or stirring that creates bubbles
• Application of paint on a highly porous surface that has not been previously primed
• Application of the paint at extremely high temperatures

Sand the surface with No80 sandpaper until the paint is removed. Then, repair any problems on the substrate if present, and prime using SOLVENT-BASED PRIMER (The SOLVENT-BASED PRIMER is thinned with DUROSTICK’s THINNER 101. Strictly follow the dilution and usage instructions stated in the product’s TDS) or with AQUAFIX.

Next, repaint the surface using the acrylic paint 10 YEARS WARRANTY, 100% ACRYLIC PAINT, or another exterior paint by DUROSTICK.

For interior surfaces, select the ecological emulsion paint SUPER ECO or the emulsion paint EXTRA.

Solvent Based Primer Stabilizer for plaster, concrete, drywall & cement boards View more
Thinner 101 Enamel paint thinner View more
Aquafix
Aquafix Micromolar stabilizer for walls, roofs & drywall View more
10 Years Warranty 100% Acrylic paint View more
100% Acrylic Top quality acrylic paint View more
SUPER
Super Eco Ecological emulsion paint for indoor use View more
Extra Highly durable emulsion paint View more
×

    TECHNICAL SUPPORT

    The specialized Technical Support department, with experienced engineers, is always available to solve your questions or technical issues.

    This site is registered on wpml.org as a development site. Switch to a production site key to remove this banner.