Paint cracking on exterior surfaces

Discover the potential causes and view the solutions
• Excessively thinned paint
• The surface was not primed

Prepare, fill/skim coat, prime, and paint as described in the previous section “Peeling paint on exterior surfaces”, strictly following the usage and dilution instructions printed on the product packaging.

• Application of paint at improper thicknesses
• Application of paint on surfaces where the primer had not been thinned
• Problematic plaster or skim coat substrate
• Application of paint on a surface where proper preparation had not been carried out

Sand the surface with No80 sandpaper until the paint is removed.

Next, restore any substrate problems if present and waterproof with WATERPROOF MORTAR, creating a stable and waterproof substrate for the final decorative paint coat.

Prime with SOLVENT-BASED PRIMER (The SOLVENT-BASED PRIMER is thinned with DUROSTICK’s THINNER 101. Strictly follow the dilution and usage instructions stated in the product’s TDS) or with the micromolecular stabilizer AQUAFIX.

Repaint the surface with the acrylic paint 10 YEARS WARRANTY or with the elastomeric waterproofing paint D-80 HYDROSTOP ELASTIC.

WATERPROOF_MORTAR
Waterproof Mortar Flexible waterproofing mortar for wall surfaces View more
Solvent Based Primer Stabilizer for plaster, concrete, drywall & cement boards View more
Thinner 101 Enamel paint thinner View more
Aquafix
Aquafix Micromolar stabilizer for walls, roofs & drywall View more
10 Years Warranty 100% Acrylic paint View more
D80_15kg
D-80 Hydrostop Elastic Elastomeric and sealing paint View more
×

    TECHNICAL SUPPORT

    The specialized Technical Support department, with experienced engineers, is always available to solve your questions or technical issues.

    This site is registered on wpml.org as a development site. Switch to a production site key to remove this banner.